Here are the applicable specifications:

QQ-N-290A

There is a nickel finish for almost any need. Nickel can be deposited soft or hard-dull or bright, depending on process used and conditions employed in plating Thus hardness can range from 150-500 Vickers Can be similar to stainless steel in color, or can be a dull grey (almost while) color. Corrosion resistance is a function of thickness. Has a low coefficient of thermal expansion. Is magnetic. All steel parts having a hardness of RC-40 or greater require a post bake at 375°F ±25° for 3 hours.

NOTE: All steel parts having a tensile strength of 240,000 or greater shall not be nickel plated without specific approval of procuring agency.

Type Class Thickness Comments
Class 1 .0016" For corrosion protection. Plating shall be applied over an underplating of copper or yellow brass on zinc and zinc-based alloys. In no case shall the copper underplate be substituted for any part of the specified nickel thickness.
.0012"
.0010"
.0008"
.0006"
.0004"
.0002"
Class 2
For engineering applications.